Laboratory Findings of Silver-Titanium Implants
[Bacteria Staphylococcus aureus (MRSA +)]
Picture 1
Picture 2
[Picture 1] The Titanium disc contamined with Staphylococcus aureus (MRSA +) and cultured on agar. It shows the spreading of the bacteria on the disc place with collonisation. Temp: 37°, duration 12 hours.[Picture 2] The Titanium-Silver disc contamined with Staphylococcus aureus (MRSA +) and cultured on agar. It shows no spreading of the bacteria on the disc place and no any collonisation. Temp: 37°, duration 12 hours.
[Picture 3] The half of disc made from Titanium and the other half is
made from Titanium-Silver. The all agar contamined with Staph.
aureus and then the disc puted on it. After 12 hours at 37° there is
no spreading of the bacterial collony on the Titanium-Silver area.[Picture 4] The disc made from Titanium. The all agar contamined
with Staph. aureus and then the disc puted on it. After 12 hours at
37° there is much more spreading of the bacterial collony on the
Titanium and agar area.
Postop Deep Wound Infection Of The Lung Cancer Patient After Normal Titanium Screw Implants
Bacterial Culture Showed [Staphylococcus aureus MRSA (+)]
Pre-op / Post-op Infection Pictures
There are wound infection after Normal Titanium Spinal Implant Application on the Cancer Patient [Picture 1]. This wound showed MRSA (+) infection via culture [Picture 2].
The first Spinal System Removed from Patient and Applied Antibacterial Silver Covered Spinal System [Picture 3]. Wound Closed [Picture 4].

Staphylococus (MRSA)
Products...
Refferences...
Laboratory Works...
Clinical Effects...
Distributors...
Distributors in the world of antibacterial silver-coated Titanium Spinal System...
Would you like to be distributor?